[labnetwork] Looking for PFA or PTFE carriers for thicker wafers
Lino Eugene
lino.eugene at uwaterloo.ca
Fri Jan 7 11:59:18 EST 2022
Hi Jeffrey,
ePAK modifies their standard wafer cassettes by removing teeth to make the slots larger. It is probably the same process for other companies.
They can modify their standard PFA cassette eWB0309. You need to make sure that the outline fits with your SRD.
Best,
Lino Eugene, P.Eng., Ph.D.,
Micro/nanofabrication process engineer
Quantum Nano-Fabrication and Characterization Facility
QNC 1611
University of Waterloo
200 University Avenue West
Waterloo, ON, Canada
N2L 3G1
Ph: +1 519-888-4567 #37788
Cell: +1 226-929-1685
Website: https://qnfcf.uwaterloo.ca/
From: labnetwork [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Salzmann, Jeffrey
Sent: January 6, 2022 13:10
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] Looking for PFA or PTFE carriers for thicker wafers
Hello!
I am working with 100mm wafers, but they’re up to 2mm thick (versus the standard 525/625µm).
Does anyone have a recommendation or contact I could use to procure these?
Thanks!
Jeff
Jeff Salzmann
Senior Research Engineer
Advanced Materials Technology Group
Integer*
10000 Wehrle Drive
Clarence, NY, 14031
Tel +1 716.759.5796
Cell +1 716.867.1302
Jeffrey.Salzmann at integer.net<mailto:Jeffrey.Salzmann at integer.net>
www.integer.net<http://www.integer.net/>
* Integer comprises the following companies:
Greatbatch Medical -‐ Lake Region Medical -‐ Electrochem
________________________________
Integer Confidentiality Notice: This electronic mail transmission is intended for the use of the individual or entity to which it is addressed and may contain confidential or proprietary information belonging to the sender. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, or the taking of any action in reliance on the contents of this information is strictly prohibited. If you have received this transmission in error, please notify the sender immediately by e-mail and delete the original message. Thank you for your cooperation.
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20220107/3051981c/attachment.html>
More information about the labnetwork
mailing list