[labnetwork] Benchtop plating or plating service
Price, Aimee
price.798 at osu.edu
Mon Oct 31 11:10:31 EDT 2022
Hello labnetwork,
We have a collaborator who needs to plate a few (2-4um) of Au. We do not maintain a plating setup here at Ohio State.
Does anyone have recommendations for a benchtop plating setup (i.e. not a standalone plating bath/bench)? They have a completely available fume hood that could be used if there was a good option.
Alternatively, does anyone do this as a service?
Thank you,
Aimee Bross Price
Manager, Nanofabrication
The Ohio State University
Nanotech West Lab
Institute for Materials Research
1381 Kinnear Road
Suite 100
Columbus, OH 43212
614-292-2753