Hi Aimee,
We have a gold plating station here at the LNF and offer remote processing
services. Our Au plating solution is BDT-510.
If your collaborator is interested, please have them reach out to us at
info at lnf.umich.edu.
Please let me know if you have any questions.
Thanks, Rob
On Mon, Oct 31, 2022 at 11:48 AM Price, Aimee <price.798 at osu.edu> wrote:
> Hello labnetwork,
>
> We have a collaborator who needs to plate a few (2-4um) of Au. We do not
> maintain a plating setup here at Ohio State.
>
>
>
> Does anyone have recommendations for a benchtop plating setup (i.e. not a
> standalone plating bath/bench)? They have a completely available fume hood
> that could be used if there was a good option.
>
>
>
> Alternatively, does anyone do this as a service?
>
>
>
> Thank you,
>
> Aimee Bross Price
>
>
>
> Manager, Nanofabrication
>
> The Ohio State University
>
> Nanotech West Lab
>
> Institute for Materials Research
>
> 1381 Kinnear Road
>
> Suite 100
>
> Columbus, OH 43212
>
> 614-292-2753
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
--
Robert Nidetz, PhD (he/him/his)
University of Michigan
LNF User Liaison and Domain Expert
1241 EECS Building
1301 Beal Ave
Ann Arbor, MI 48109
nidetz at umich.edu
734.496.8065
Book an appointment: https://calendly.com/nidetz
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20221031/811894f8/attachment.html>
More information about the labnetwork
mailing list