[labnetwork] Ti Sputtering with a Lesker Torus MagKeeper without a backing plate
Carsen Kline
carsen at stanford.edu
Tue Aug 15 17:35:48 EDT 2023
Hi Tucson,
Except for extremely hard (W, Mo) or brittle materials (pressed powder oxides or nitrides), our MagKeeper targets are directly drilled and tapped with a single hole to attach the keeper button, no backing plate needed. Our target vendor provides this service and will also retrofit non-keeper targets in their machine shop.
I would not attempt to run a non-keeper target on a MagKeeper gun, especially if it's inclined at an angle.
Cheers,
Carsen
SNF
________________________________
From: labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Richelson, Tucson <tucsonr at illinois.edu>
Sent: Tuesday, August 15, 2023 9:16 AM
To: 'labnetwork at mtl.mit.edu' <labnetwork at mtl.mit.edu>
Subject: [labnetwork] Ti Sputtering with a Lesker Torus MagKeeper without a backing plate
Hello all,
I have a Lesker PRO-Line Sputter tool and the guns have Torus MagKeepers. I have a student that would like to sputter Ti. I have a Ti target, but it doesn’t have a backing. All of my other targets have backings. It seems logical that if I want to use a target on a gun with a MagKeeper I would need a backing (pictured is my Al target with a backing).
I asked our Lesker sales rep and his response was to use the Ti target without the backing. I asked if the target will slide off of the gun. His response was no.
Does this make sense? Does anyone have experience with sputtering Ti in a Lesker tool?
[cid:image001.png at 01D9CF69.BC18FC10]
Best,
Tucson Richelson
-------------------------------------------------------------------------
Nick Holonyak, Jr. Micro and Nanotechnology Lab (HMNTL)
University of Illinois
Rm 2118, MC-249
208 North Wright St. Urbana, IL 61801
Office: +1 (217) 244-5138
Web: http://mntl.illinois.edu/
Schedule training: https://book.ms/b/Training2@uillinoisedu.onmicrosoft.com
Under the Illinois Freedom of Information Act any written communication to or from university employees regarding university business is a public record and may be subject to public disclosure.
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230815/c6b22319/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 11105 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230815/c6b22319/attachment.png>
More information about the labnetwork
mailing list