I use Brewer Science, XHRiC I-line Anti Reflective Coating.
See:
https://wiki.nanotech.ucsb.edu/wiki/images/3/33/XHRiC-Anti-Reflective-Coating.pdf
See also:
H. Northfield, O. Krupin, R. N. Tait, and P. Berini, “Tri-layer contact photolithography process for high-resolution lift-off,” Microelectron. Eng. 241 (2021).
Howard Northfield
Research Associate
Advanced Research Complex (ARC)
University of Ottawa
________________________________
From: labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Bikash Dev Choudhury <d.c.bikash at iitb.ac.in>
Sent: Friday, June 23, 2023 5:26 AM
To: labnetwork at mtl.mit.edu <labnetwork at mtl.mit.edu>
Subject: [labnetwork] Antireflective coating for Litho process
Attention : courriel externe | external email
Dear Labnetwork,
I am looking for antireflective coating for both top and bottom layer in photolitho process.
Looking forward for any lead/info.
Thanks in advance!
--
Best Regards
Dr. Bikash Dev Choudhury
Sr. Process Technologist
CEN, IITBNF
Electrical Engineering Department
IIT Bombay, Mumbai-400076
Mobile No. 7400319871
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230623/416d3061/attachment.html>
More information about the labnetwork
mailing list