Dear Lab Network,
I was wondering how long the lifetime is for the HMDS in the YES oven. On
the note from the YES's website, it says " If the HMDS is more than a year
old, it should probably be replaced". I would assume the "year" here starts
from the HMDS manufactured date, which is the shelf life for a brand new
bottle of HMDS. Do you guys have experience on using the HMDS for extended
time (like 6+ months) after the expiration date? Please let me know your
thoughts and suggestions. Many thanks!
Best,
Chao
--
*Zhichao "Chao" Wang, Ph.D.*
*Lithography Engineer*
*UDNF*
*University of Delaware*
*Pronouns: He/Him/His*
*------------------------*
*Office Number:(302) 831-4839*
*221 Academy St.,RM170*
*Newark, DE 19711*
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20240408/586fe4ca/attachment.html>
More information about the labnetwork
mailing list