For one of our outreach events we print user’s images onto transparencies,
for litho on an MA6.
However we often run into the problem that for some combination of
transparencies and printer ink, the ink just rubs right off the plastic
transparency, even if left to dry for hours!
We believe that the same transparencies that worked last year, this year
had the ink rub off. Do we need to vac seal the transparencies when unused?
If anybody knows what the combo is that works/fails, your advice would be
greatly appreciated.
-- Demis
----------------------------------------
* Process Group Manager*
*UCSB Nanofabrication Facility* <https://www.nanotech.ucsb.edu/>
Demis' Contact Info
<https://wiki.nanotech.ucsb.edu/wiki/Demis_D._John>
----------------------------------------
*Reminder*: The NanoFab has a publications policy
<https://wiki.nanotech.ucsb.edu/wiki/Frequently_Asked_Questions#Publications_acknowledging_the_Nanofab>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20240129/d5581668/attachment.html>
More information about the labnetwork
mailing list