[labnetwork] OXford Plasmalab System 100 (ICP-RIE) - PCB BOARD ISSUE
Christophe Clément
christophe.clement at polymtl.ca
Tue Mar 19 09:03:21 EDT 2024
Hello community
We recently had a water leak on our ICP-RIE Plasmalab System100 (an
ICP-RIE). Water went on the main PCB board without touching the X20 PLC by
chance.
We could not have +24 +15 and -15VDC on screen to restart all pumps. After
some work on the PCB board we could find a faulty resistor and could
finally restart the pumping, but still some issues were still present (no
CM Gauge reading on the software, and some heaters at max temperature).
After some step forwards, we did step backwards because now we have lost
the communication between PC and PLC.
We have then decided to ask Oxford for a PCB replacement (94-PC91S21083
REV 3), but what we received is not what we were expecting (I did not know
if I had to laugh or cry when opening the box
)
Left: what we need, right: what we received from Oxford.
If some Oxford tool owners, or any refurbished equipments company, or any
third party company that works with Oxford tools read this message and
know where we can buy a refurbished 94-PC91S21083 REV 3 PCB board or offer
any advice, that will be greatly appreciated!
Thank you
Christophe
Christophe Clément
Professionnel de recherche
Laboratoire de microfabrication (LMF)
Groupe des Couches Minces (GCM) <http://www.gcmlab.ca/> www.gcmlab.ca
Ecole Polytechnique de Montréal <http://www.polymtl.ca/> www.polymtl.ca
Département de génie physique
* 2900 Boulevard Edouard Monpetit
Pavillon JAB
Campus de l'Université de Montréal
Montréal (Québec) H3T 1J4
8 <mailto:christophe.clement at polymtl.ca> christophe.clement at polymtl.ca
( 514 340 4711 #2417
Fax : 514 340 5195
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20240319/030c1b7b/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.jpg
Type: image/jpeg
Size: 18882 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20240319/030c1b7b/attachment.jpg>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image002.jpg
Type: image/jpeg
Size: 16132 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20240319/030c1b7b/attachment-0001.jpg>
More information about the labnetwork
mailing list