[labnetwork] Dilution of Triton X-100
Aebersold,Julia W.
julia.aebersold at louisville.edu
Fri Aug 10 17:06:38 EDT 2012
We purchase both, BHF with and without surfactant pre-mixed in it.
Cheers!
Julia Aebersold, Ph.D.
MNTC Cleanroom Manager
Shumaker Research Building, Room 233
2210 South Brook Street
University of Louisville
Louisville, KY 40292
502-852-1572
http://louisville.edu/micronano/
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Morrison, Richard H., Jr.
Sent: Thursday, August 09, 2012 11:10 AM
To: Fouad Karouta; labnetwork at mtl.mit.edu
Subject: Re: [labnetwork] Dilution of Triton X-100
Here at Draper we dilute it with water, or if you are adding it to the BHF then you want 1% of the total volume to be TritonX-100, just premix it in water and then add that. It takes some time to get the Triton X-100 to mix into the water.
Why not just buy the BHF with a surfactant already mixed in. Transene Company can do this for you.
Rick
Rick Morrison
Senior Member Technical Staff
Group Leader Microfabrication Operations
Draper Laboratory
555 Technology Square
Cambridge, MA 02139
W 617-258-3420
C 508-930-3461
From: labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu> [mailto:labnetwork-bounces at mtl.mit.edu]<mailto:[mailto:labnetwork-bounces at mtl.mit.edu]> On Behalf Of Fouad Karouta
Sent: Thursday, August 09, 2012 3:33 AM
To: labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
Subject: [labnetwork] Dilution of Triton X-100
Hello all,
Recently when discussing with Bill Flounders about adding a surfactant to BHF solution he suggested to use Triton X-100.
We like to use it in a diluted form. From internet I could find water, toluene, xylene and ethanol can be used as diluent. However water may turn the solution gelatinous.
Does anyone have experience with diluting triton x-100 (supplier Sigma Aldrich)?
Thanks,
Fouad Karouta
*********************************
Facility Manager ANFF ACT Node
Research School of Physics and Engineering
Australian National University
ACT 0200, Canberra, Australia
Tel: + 61 2 6125 7174
Mob: + 61 451 046 412
Email: fouad.karouta at anu.edu.au<mailto:fouad.karouta at anu.edu.au>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20120810/21ef3330/attachment.html>
More information about the labnetwork
mailing list