[labnetwork] cleaning sulfur from DRIE coldtrap
Mark Morgan
mmorgan3 at uw.edu
Wed Jun 1 14:00:24 EDT 2016
Greetings all -
is there a preferred procedure for cleaning sulfur deposits from a DRIE cold trap and unheated length of roughing line? i am reticent to apply a ‘brute-force’ method when a more elegant solution is available (and perhaps using the word ‘elegant’ regarding sulfur cleaning is mis-guided…) but even still, i am open to suggestions.
thank you so much
best regards
Mark
Mark D. Morgan
Research Engineer, Washington Nanofabrication Facility (WNF)
National Nanotechnology Coordinated Infrastructure (NNCI)
University of Washington
Fluke Hall 132, Box 352143
(206) 221-6349
mmorgan3 at uw.edu <mailto:mmorgan3 at uw.edu>
http://www.wnf.washington.edu/ <http://www.wnf.washington.edu/>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20160601/6da8d2fd/attachment.html>
More information about the labnetwork
mailing list