[labnetwork] HF Vapour Setup
Frank Dirne - TNW
F.W.A.Dirne at tudelft.nl
Tue May 22 03:04:23 EDT 2018
Idonus has a similar set-up.
Recently we had a failure in the electrostatic chuck and after returning it to Idonus we had a repaired chuck within 7 working days.
best regards / met vriendelijke groeten,
Frank Dirne
Managing Director Kavli Nanolab
Delft University of Technology
Lorentzweg 1, 2628 CJ Delft
TNW (bldg 22) - room D121
Phone: +31 (0)15 27 82357 / +31 614330507
email: F.W.A.Dirne at tudelft.nl<mailto:F.W.A.Dirne at tudelft.nl>
secretary: +31 (0)15 27 82898
website: www.qn.tudelft.nl/KN<http://www.qn.tudelft.nl/KN>
[cid:BE01F5A2-838B-40F8-A7BA-0A109001FFB3]
Fank Dirne
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Fouad Karouta
Sent: maandag 21 mei 2018 5:00
To: labnetwork at mtl.mit.edu
Subject: [labnetwork] HF Vapour Setup
Dear all,
We have an AMMT HF vapour setup for up to 4 " wafer size.
Recently we are experiencing problems not being able to apply a voltage on the electro-static chuck to hold the wafer. We tried to contact AMMT in Germany (2 emails and 3 phone calls talking with an administrator) but we never got any feedback/reply from an engineer.
Has anyone experience with HF vapour setup? I wonder if someone has established contacts with someone from AMMT.
Also has anyone good experience with other possible suppliers of HF vapour setup?
Thank you,
Fouad Karouta
*************************************
Manager ANFF ACT Node
Australian National Fabrication Facility
Research School of Physics and Engineering
L. Huxley Building (#56), Mills Road, Room 4.02
Australian National University
ACT 2601, Canberra, Australia
Tel: + 61 2 6125 7174
Mob: + 61 451 046 412
Email: fouad.karouta at anu.edu.au<mailto:fouad.karouta at anu.edu.au>
http://anff-act.anu.edu.au/
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180522/8abab12f/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 17854 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20180522/8abab12f/attachment.png>
More information about the labnetwork
mailing list