[labnetwork] How to charge for sputtering target use
Aebersold,Julia W.
julia.aebersold at louisville.edu
Fri Jun 5 11:12:29 EDT 2020
We have shared targets and remove them after each use. Clients weigh the targets before and after each use for precious metals only, but for cheaper materials like aluminum the material is included in the cost of running the sputterer.
Cheers!
Julia Aebersold, Ph.D.
Manager, Micro/Nano Technology Center
University of Louisville
Shumaker Research Building, Room 233
2210 South Brook Street
Louisville, KY 40292
(502) 852-1572
http://louisville.edu/micronano/
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Michael Dimitri Sinanis
Sent: Thursday, June 4, 2020 8:20 PM
To: Chang, Long <lvchang at Central.UH.EDU>; labnetwork at mtl.mit.edu
Subject: Re: [labnetwork] How to charge for sputtering target use
CAUTION: This email originated from outside of our organization. Do not click links, open attachments, or respond unless you recognize the sender's email address and know the contents are safe.
Long,
One method that I have used in a similar situation is as follow:
1. Target with cost A installed (Cost AA, weight WW)
2. User 1 sputters 2 microns
3. User 2 sputters 1 micron
4. User 3 sputters 4 microns
5. User ............... (and so on)
6. Target A has been consumed and replaced with Target H
7. Target A (what is remaining) is reclaimed in dollars (Cost BB, weight XX)
Cost used = Cost AA - Cost BB
Metal used = Weight WW - Weight XX
Total microns sputtered = User 1 + User 2+ ......
Cost per micron used = Cost used / Total microns sputtered
Cost per metal used = Metal used / Total microns sputtered
If one target tends to take longer than a fiscal year to be consumed than I would use the market price per weight.
If the target tends to get consumed within a few months then I would use the cost per micron from the previous cycle to charge the use today.
Of course this is not perfect, but it gives you a fair baseline I think.
Best,
Michael
________________________________
From: labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu> <labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu>> on behalf of Chang, Long <lvchang at Central.UH.EDU<mailto:lvchang at Central.UH.EDU>>
Sent: Thursday, June 4, 2020 11:50 AM
To: labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu> <labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>>
Subject: [labnetwork] How to charge for sputtering target use
Hi All,
At UHNF, each user owns their own sputtering target. We are currently considering a shared model for expensive targets like Au, Pt, etc. Does anyone have a reasonable way to estimate material usage vs something we can track so that we can charge fairly? What approaches do y'all take to manage how expensive material is shared?
Thanks,
Long
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20200605/351ae43e/attachment.html>
More information about the labnetwork
mailing list