[labnetwork] Plasmatherm Apex ICP High Temperature Operation
Jeremy Clark
clark at cnf.cornell.edu
Wed Jun 23 16:20:15 EDT 2021
The trick with the dots is that you need to press them hard and flat to
the wafer, as the vacuum tries to pull them up and away from the
surface, thus defeating the purpose of measuring the temperature of a
surface.
Also leave the wafer in there for a few minutes- or wait /and/ don't
wait with separate dots and see the difference!
Jeremy Clark
Cornell Nanoscale Facility
On 6/23/21 1:16 PM, LaFleur, David W wrote:
>
> Hi Bruce
>
> There are 2 ways I know of, an inexpensive way and an expensive way.
> The inexpensive way is to use thermal dots sold here:
>
> https://www.mcmaster.com/temperature-indicating-dots/
> <https://www.mcmaster.com/temperature-indicating-dots/>
>
> Expensive way is using SensArray.
>
> https://www.kla-tencor.com/products/chip-manufacturing/in-situ-process-management
> <https://www.kla-tencor.com/products/chip-manufacturing/in-situ-process-management>.
>
> Regards,
>
> Dave LaFleur
>
> Harvard University
>
> CNS
>
> *From: *"labnetwork-bounces at mtl.mit.edu"
> <labnetwork-bounces at mtl.mit.edu> on behalf of Bruce Tolleson
> <betemc at rit.edu>
> *Date: *Wednesday, June 23, 2021 at 11:42 AM
> *To: *"labnetwork at mtl.mit.edu" <labnetwork at mtl.mit.edu>
> *Subject: *[labnetwork] Plasmatherm Apex ICP High Temperature Operation
>
> Dear Labnetwork,
>
> Our Plasmatherm Apex ICP has the high temperature option installed
> to run as high as 200°C. We are trying to determine the actual
> temperature of the lower electrode to substrate contact. The display
> temperature verses actual temperature has an offset and we are trying
> to determine what that offset is. Has anyone else been able to measure
> this?
>
> Thank you,
>
> Bruce E. Tolleson
>
> Rochester Institute of Technology
>
> 82 Lomb Memorial Drive, Bldg 17-2627
>
> Rochester, NY 14623-5604
>
> (585) 478-3836
>
> http://www.rit.edu/~962www/logos/tiger_walking_rit_color.jpg
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20210623/8aa68f9b/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.jpg
Type: image/jpeg
Size: 2551 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20210623/8aa68f9b/attachment.jpg>
More information about the labnetwork
mailing list