[labnetwork] old SensArray Corp wafers & wiring/connectors
Kyle Keenan
kckeenan at seas.upenn.edu
Mon Jan 23 08:55:04 EST 2023
Hi Steve,
Thanks for your input. They have multipoint capability, and the connectors
are big and clunky with a lot of wires. I'll let you know if we end up not
using them.
Best,
Kyle
On Fri, Jan 20, 2023 at 5:12 PM Paolini, Steven <
spaolini at cns.fas.harvard.edu> wrote:
> Kyle,
>
> Those SensArray wafers are valuable tools. You don’t need a fancy
> dedicated temp reader for them, a simple digital thermometer or DVOM with a
> T/C input will do unless you need to map across the wafer simultaneously.
> As long as the reading instrument has the same T/C type as the junctions on
> the wafer, it should work just fine. These are critical tools for checking
> wafer temps in a vacuum system (the flat leads are designed to cross an
> Oring) or an RTP. If you have no use for them, I would be interested in
> purchasing them from you.
>
> As always, best regards,
>
> Equipment Dood
>
>
>
> Steve Paolini
>
> Principal Equipment Engineer
>
> Harvard University Center for Nanoscale Systems
>
> 11 Oxford St.
>
> Cambridge, MA 02138
>
> 617- 496- 9816
>
> spaolini at cns.fas.harvard.edu
>
> www.cns.fas.harvard.edu
>
>
>
> *From:* labnetwork <labnetwork-bounces at mtl.mit.edu> * On Behalf Of *Kyle
> Keenan
> *Sent:* Friday, January 20, 2023 3:21 PM
> *To:* Lab Network (labnetwork at mtl.mit.edu) <labnetwork at mtl.mit.edu>
> *Subject:* [labnetwork] old SensArray Corp wafers & wiring/connectors
>
>
>
> Hello All,
>
>
>
> I'm wondering if any of you have any experience with SensArray products
> from the early 2000's. I have a couple of wire & connector sets (p/n
> 1410-0-5103Z) complete with 3.5" floppy disk software, no less, plus a
> handful of 6" temp mapping wafers (2210's), as well as one 8" wafer. Some
> of this stuff looks like it's never been used, but I don't know much about
> it and whether or not it's worth keeping, particularly since I have no temp
> reader.
>
>
>
> Please let me know your thoughts.
>
>
>
> Thank you,
>
> --
>
> Kyle Keenan
>
>
>
> Senior Manager - Laboratory Operations
>
> Quattrone Nanofabrication Facility
>
> University of Pennsylvania
>
> P: 215-898-7560
>
> F: 215-573-4925
>
--
Kyle Keenan
Senior Manager - Laboratory Operations
Quattrone Nanofabrication Facility
University of Pennsylvania
P: 215-898-7560
F: 215-573-4925
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230123/d960256e/attachment.html>
More information about the labnetwork
mailing list